Abstract

The Main Purpose Of This Paper Is To Reduce The Casting Defects By Analyzing And Detecting With The Use Of Nondestructive Testing Methods. In Most Of The Industries As We All Are Aware About The Normal Casting Defects Which Are Generated During The Po


Keywords

Chaplets Core Print Cores Die Casting Foundry Green Molding Sand & Casting Defects.

Paper ID

IJSARTV3I28360

Publication Date

February 18, 2017

Research Area

Mechanical Engineering

Submit Your Paper to IJSART

Join the global research community with IJSART. Submit your paper, share your work, and gain worldwide recognition!